Skip to content
  • There are no suggestions because the search field is empty.

What is the installation process with mortar and mesh treatment in joints?

Indications on how to do the joint treatment and considerations.

After leaving a spacing of 3-5mm when fixing the boards, fill all joints with AQUAPANEL® Joint Filler & Skim Coating – white, and then embed AQUAPANEL® Tape (10 cm) centered over all joints. Apply a thin layer of AQUAPANEL® Joint Filler & Skim Coating – white to cover the tape. Expansion joints should be at a max. of 15 m intervals.